HP200 Quaternized Wheat Protein Specifications, Performance and Uses

HP200 is an aqueous blend containing Cocodimonium Hydroxypropyl Hydrolyzed Wheat Protein, unmodified Hydrolyzed Wheat Protein, water and Phenoxyethanol. It is intended for hair-care projects where protein-derived conditioning and film formation are of interest.

Technical specifications

Parameter Value
Appearance Clear amber liquid
Quaternized wheat protein component ≥40.0%
Hydrolyzed Wheat Protein ≤12.0%
Phenoxyethanol 0.6–0.8%
Dry residue ≥50.0%
pH 4.0–7.0 in a 1.0% solution

The dry residue measures total residue. Use the separate composition entry for the quaternized component and count the Phenoxyethanol contributed by the raw material in the full formula.

Performance and formulation functions

The supplier TDS describes hair conditioning, film formation and easier combing. Wang et al. prepared a separate quaternized wheat protein hydrolysate and studied its interaction with hair in model shampoos. The results explain why this ingredient family is of interest for conditioning. They apply to the materials and formulations studied. Measure HP200 combability, feel and appearance in the intended formula.

Applications and use guidance

The TDS lists shampoos, conditioners, styling products and hair sprays. Its reference inclusion range is 0.50–5.0% of the commercial blend, and it suggests addition around 80°C in shampoo and conditioner trials. Check addition order, heat exposure and color or haze against the base before setting the manufacturing procedure.

What quaternization changes in a wheat protein hydrolysate

Hydrolysis produces a mixture of smaller peptides. Quaternization introduces positively charged groups that can favor interaction with negatively charged hair surfaces. Wang and colleagues prepared a quaternized wheat protein hydrolysate and compared it with an unmodified hydrolysate and a cationic cellulose comparator. Their work included uptake and combing measurements. The study provides an experimental basis for comparing modified and unmodified proteins. The researchers’ preparation and test system had their own composition, so the results describe that material and do not quantify the effect of HP200. Original wheat protein modification and hair-conditioning study.

Account for protein fractions and preservative

HP200 is supplied as a mixture. In a 100 g illustrative prototype containing 2.00 g of HP200, the supplier limits imply at least 0.80 g of quaternized hydrolysate, up to 0.24 g of unmodified hydrolysate and 0.012–0.016 g of phenoxyethanol. The residue specification translates to at least 1.00 g of material under the TDS test conditions. Total residue and quaternized protein content describe different measurements. Use the grade assay when an experiment requires equal quantities of protein and account for the phenoxyethanol already present when assessing the finished formula’s preservative system.

Design a test that isolates the effect of the protein

For a conditioner or mask, start with the existing base at constant oil, fatty alcohol and main cationic surfactant levels. Compare the base, a carrier and preservative control where feasible, and the HP200 prototype. To test the role of quaternization, add a separate unmodified wheat hydrolysate comparator at a defined protein basis if compositional information is available. Match final pH and water content across the samples. Use the same tress weight, treatment quantity, contact time and rinse procedure.

Use wet combing work for detangling and a blinded sensory assessment for dry feel. Consider testing damaged and untreated hair as separate groups. Track appearance, odor, pH and viscosity through storage, and monitor repeated-use feel before attributing a benefit to additional deposition. If the target is a shampoo, check haze and sediment in the concentrate and during dilution with the intended anionic system. These measurements support claims about the specific performance observed, such as easier combing under the chosen conditions. Tensile strength or breakage claims call for dedicated mechanical tests.