Polyquaternium-28: Relating Film Properties to Humidity-Exposed Hair Performance
Question
Does a PQ-28 styling prototype preserve the desired shape under humidity without unacceptable tack, flaking or loss of movement? A polymer film can look strong on glass while behaving differently on a curved, porous hair substrate. The study therefore needs both a reproducible cast-film phase and a matched-tress phase.
Read the TDS in context
The PQ-28 grade sheet lists Polyquaternium-28, solids 19–21%, pH 5–8 for a 1% aqueous solution at 25 °C and typical raw-material viscosity 20,000–60,000 mPa·s at 25 °C. The document notes typical data are not intended to set specifications. A 0.50 g as-supplied dose to a 100 g batch contributes 0.095–0.105 g total solids based on the range. That does not define pure polymer content, charge equivalents or use level. Confirm lot assay and composition before making a precise active-matter comparison.
Film properties and environment
Film-forming polymer mechanics can change with moisture. Controlled-humidity dynamic mechanical analysis has been used to examine personal-care polymer films, while dynamic-humidity curl-retention research uses tresses and humidity steps. These methods inform a design that measures film response and hair-shape response separately. They do not provide a PQ-28 performance prediction unless the grade itself was tested under the same vehicle and conditions. Humectant, plasticizer, residual water and dry-film mass can all change tack or flexibility, so hold them constant in the first screen.
Cast-film protocol
Prepare vehicle control and at least two PQ-28 solids levels in the same base. Cast equal wet mass over the same area on a defined substrate. Dry at controlled temperature and humidity until mass is stable, then condition samples at at least two controlled relative-humidity points. Measure tack or probe adhesion, bend response and visual whitening using a prespecified method. Include replicate casts from independently prepared batches. If equal wet application yields different dry film mass, add a second comparison normalized to dry mass; these answer different questions.
Tress application and curl retention
Use tresses from one source and stratify by initial curl response. Standardize cleansing, initial moisture, product mass per gram of hair, applicator, roller diameter, drying and conditioning time. Randomize coded tresses among the vehicle, candidate and reference. Record initial curl length L0, straightened reference length Ls and hanging length Lt at defined intervals during humidity exposure. Calculate retention as 100 × (Ls − Lt)/(Ls − L0), and exclude tresses with an unstable or very small denominator under a predefined rule. Report each tress and uncertainty rather than just a mean.
Environmental design
Log actual temperature, relative humidity, equilibration time, airflow and chamber position. A useful stress screen can include a laboratory baseline, a high-humidity exposure and a return to baseline to observe recovery; select exact setpoints based on the product brief and equipment validation. Prevent condensation, which creates liquid-water exposure rather than a humidity-only challenge. Photograph at fixed distance with a scale. At each time point record curl length, visible frizz, tack between fibers, flakes after a fixed number of comb strokes and subjective feel with blinded codes.
Decision logic
If initial curl formation is weak, examine application coverage and dry-down before raising polymer solids. If initial shape is comparable but high-humidity retention falls with tack, test humectant or plasticizer changes in a separate factorial block. If retention is acceptable but brushing produces flakes, hold solids and drying constant while investigating film flexibility and adhesion. If cast films appear sound but tresses fail, prioritize the hair substrate and application method rather than treating the glass result as a proxy. State findings only for the tested formula and hair set.
References and applicability
- Plant Chain PQ-28 grade documents. Supplier documents should be checked for current assay and method.
- Bayersdoerfer et al., Dynamic Humidity Curl Retention. Research group record describing humidity-step tress assessment with model polymers.
- Ferrar et al., High Humidity Mechanical Properties of Film Forming Polymers. Primary controlled-humidity film-mechanics work; polymer composition differs from this commercial PQ-28 grade.